JOURNAL HEAD RE-CONDITIONING

Industry Type

Product Group

Our solution
Product

LOTHERME-468

Size (mm)

4

Current (AMPs)

90-120

Qty. (Kgs)

20 Kg.

Product

LOTHERME OA- 352

Size (mm)

2.4

Current (AMPs)

250-300

Qty. (Kgs)

100 Kg.

Product

LOTHERME OA- 611

Size (mm)

2.4

Current (AMPs)

250-300

Qty. (Kgs)

20 Kg.

JOB PICTURES
Before
After
ANALYSIS
EQUIPMENT

SUPRA MMA 630-T

COMPONENT NAME

JOURNAL HEAD – 1 NO

TYPE OF PROBLEM

WORNOUT OF PROFILE

PROBLEM DUE TO

IMPACT & CORROSION

BASE METAL

CAST STEEL

COMP. WEIGHT (Kgs)

3T

DIM ENSIONS (mm) L x Dia

2500 x 400

Procedure

1. GRIND THE SURFACE AREA OF JOURNAL HEAD TO REMOVE FATIGUED METAL

2. DRAW THE BUFFER LAYER WITH LOTHERME-468

3. BUILD UP THE JOURNAL HEAD WITH LOTHERME OA-352

4. HARDFACE BY USING LOTHERME OA-611

5. INSITU WELDING.